Cuts Like a Knife … Hardness Testing Matters
In the highly competitive cutting blades industry, it is vital for the blade to have sufficient hardness to retain an edge, while too hard can cause brittle failure. When hardened materials are ground, residual heat may alter the microstructure and soften the blade edge. Testing the hardness of the cutting blades becomes challenging as indents […]