Low-Melting point metals such as zinc, lead and tin are not always easy to prepare. These metals are very soft and malleable, and attaining a scratch free finish can be challenging.  One of the more common problems during preparation of these specimens is embedding.  Embedding occurs when hard abrasive particles (or other contaminant) becomes fixed …