DiaMet Hardness Software – Weld Testing Using Vickers Hardness Scale

Welded joints are nowadays indispensable in the automotive and aviation industry. Welds usually combine metallic components to form a structure that is then assembled in production and assembly with other subassemblies. The welds must be able to withstand extreme loads as they are the weak points of the construction. Weld seam inspection is thus a …

DiaMet Hardness Software – Weld Testing Using Vickers Hardness Scale Read More »