Selection of Compression Mounting Compounds
Selection of the correct mounting compound can make all the difference in achieving high quality preparation. Edge retention compounds such as EpoMet have excellent hardness and shrinkage properties, and are best for hard materials where edge inspection is required as well as for resistance to strong chemical etches. Phenocure is the lowest cost option, and […]